Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra HS2211 BK E70405 - PA610... - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra HS2211 BK E70405:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid Terra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
High-viscosity, heat- and light-stabilized Polyamide 610 Compound for extrusion
VESTAMID® Terra HS2211 BK E70405 is a polyamide 610 compound developed for the manufacturing of tubing systems with higher demands on heat resistance.

The melting range of VESTAMID® Terra HS2211 BK E70405 is about 40°C higher than PA 11 and PA 12 compounds and allows higher peak temperatures in use.

The compound is especially suitable for the extrusion of tubing systems that are exposed to high burst pressures at high service temperatures, e.g., hydraulic clutch lines. The process temperatures should be within a range of 240°C to 270°C.

VESTAMID® Terra HS2211 is delivered as cylindrical granules ready for processing in moisture-proof packaging. 

VESTAMID® Terra HS is partly based on renewable raw materials and fills the performance gap between the commodity and the niche long-chain nylons.
VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid—S). Because sebacic acid is derived from castor oil, VESTAMID® Terra HS is a material that is partly based on bio-based and renewable resources
.

Pigmentation may affect values.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 19 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 1.6 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.3 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 2500 / - MPa ISO 527
Yield stress 66 / - MPa ISO 527
Yield strain 4 / - % ISO 527
Nominal strain at break >50 / - % ISO 527
Charpy impact strength, +23°C N / - kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Charpy notched impact strength, -30°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 222 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 42 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 54 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 155 / * °C ISO 75-1/-2
Vicat softening temperature, B 195 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 95 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 94 / * E-6/K ISO 11359-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 3.5 / * % Sim. to ISO 62
Humidity absorption 1.7 / * % Sim. to ISO 62
Density 1060 / - kg/m³ ISO 1183
Characteristics
Processing
Pipe/Tube Extrusion, Other Extrusion
Delivery form
Pellets, Granules, Black
Additives
Release agent
Special Characteristics
Light stabilized or stable to light, Heat stabilized or stable to heat
Certifications
Contains renewable resources
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.